Properties:
- semi-matte finish with a subtle gloss
- perfect hiding of layers
- rough texture
- easy to print like PLA
How to print?
The following parameters are only suggested print settings for this material. To ensure the best print quality, it is necessary to choose the appropriate settings for a specific printer and printing conditions.
Nozzle Temperature | 200-230°C |
Bed Temperature | 50°C |
Closed chamber | not required |
Fan | 75-100% |
Flowrate | 95-105% |
Printing Speed | <60 mm/s |
Surface | PEI, glass, masking tape |
Retraction (direct) | 2-3 mm |
Retraction (bowden) | 4-6 mm |
Retraction Speed | 20-45 mm/s |
Drying conditions | 40°C / 4h |
Notes | Due to the strong adhesion, damage to the bed surface (eg PEI) may occur. We recommend printing on a tape. |
Diameter | Diameter tol | Oval tol | Printing temp | Table temp |
---|---|---|---|---|
1.75 mm | +/- 0.02 mm | + 0.01 mm | 200-230°C | 50°C |
Colors

Black

Green

Blue

Red

Pink